KA518 · Automotive glass bonding

KA518 Polyurethane Windshield Adhesive

General-purpose moisture-curing adhesive for bonded windscreens, 310 ml cartridges.

Request a quote for KA518

Model
KA518
Packs
310 ml · 400 / 600 ml · 200 L / 250 kg
Tensile strength
3.5
Elongation at break
320
Technician applying polyurethane adhesive to a windscreen edge with a cartridge gun
Application example.

What it is

One-component moisture-curing polyurethane adhesive for windshield, side and rear window bonding. Good bonding and sealing, easy to apply, sag resistant, fast cure, moderate hardness after cure, water and ageing resistant, primerless.

Specification

TestStandardTypical valueMethod
Appearance — Black homogeneous paste —
Density (g/cm³) 1.5±0.1 1.50 GB/T 13477.2
Sag resistance (mm) ≤0 0 GB/T 13477.6
Skin time (min) 30–40 30 GB/T 13477.5
Cure rate (mm/day) ≥3.0 3.5 HG/T 4363
Volatile content (%) ≤5 3 GB/T 2793
Shore A hardness 60–70 65 GB/T 531.1
Tensile strength (MPa) ≥3 3.5 GB/T 528
Elongation at break (%) ≥300 320 GB/T 528
Tensile shear strength (MPa) ≥2 2.5 GB/T 7124
Extrusion rate (ml/min) ≥60 110 GB/T 13477.4

Typical values from the printed catalogue, transcribed as printed. Where the catalogue printed a unit that does not fit the value (density in g/m³), the page shows g/cm³ — see the note below.

Catalogue notes.
  • Density is printed as g/m³ in the brochure; at 1.50 the unit should be g/cm³ — a typesetting error in the original, read here as g/cm³.

Packaging

FormatSizeCarton / unit
cartridge310 ml12 / 20 / 24 pcs
sausage400 / 600 ml20 pcs
barrel200 L / 250 kg—

Where it is used

  • Bonding of windscreens, side windows and rear glass

The rest of the family

ModelDifferenceTensileElongation
KA520 Higher-modulus grade for bus and coach glazing. 4.5 450
KA530F Two-hour positioning at 23 °C with a 6.5 MPa cured tensile strength. 6.5 450

Further reading

Windscreen adhesive: the specification guide — the guide this model belongs to

Ordering. Send the model, quantity, pack format and destination — we reply with FOB/CIF pricing, lead time and the documents your customs broker will ask for. Email a quote request or write to ryan@pu-karmind.net.