Wood and glulam

One-component PUR for engineered timber, glulam beams and sandwich panels.

Choosing one

The decision is moisture and clamp time, not strength. KA505 bonds at 8–12% moisture content with 1–4 h clamp depending on temperature; wet or frozen timber foams and dry timber starves. It is not an EN 301 adhesive, so a project requiring EN 301 is asking for MUF or PRF.

Send species, moisture content and press temperature and we will return a bonding schedule. ryan@pu-karmind.net

Other families

  • Automotive glass bonding — Windscreen, side and rear glass adhesives — 310 ml cartridges, sausages and 200 L barrels.
  • Body and sheet metal — Seam sealers for body panels, doors and container joints — sandable, paintable, four colours.
  • Construction joints — Concrete, tunnel and drainage sealants — 550–615% elongation, elastic recovery up to 80%.
  • Industrial and STP — Silyl-terminated polymer sealant for metal, plastic and glass — primerless and paintable.
  • Activators and primers — Surface preparation that decides whether the bead holds: K-901 activator, K-801 primer.