KA540 · Body and sheet metal

KA540 Automotive Sheet Metal Adhesive

High-modulus seam sealer for body panels, sandable and paintable.

Request a quote for KA540

Model
KA540
Packs
310 ml · 400 / 600 ml · 200 L / 250 kg
Tensile strength
2.5
Elongation at break
600
Sealant applied along a body panel seam on a vehicle
Application example.

What it is

One-component moisture-curing high-modulus polyurethane for sheet metal seams; thixotropic, sandable and paintable, solvent-free, low VOC, non-yellowing.

Specification

TestStandardTypical valueMethod
Appearance — Black / White / Gray / Beige —
Density (g/cm³) 1.5±0.1 1.50 GB/T 13477.2
Sag resistance (mm) ≤0.5 0 GB/T 13477.6
Skin time (min) 30–60 35 GB/T 13477.5
Cure rate (mm/day) ≥3 3.5 HG/T 4363
Volatile content (%) ≤2 1 GB/T 2793
Shore A hardness 40–50 45 GB/T 531.1
Tensile strength (MPa) ≥2 2.5 GB/T 528
Elongation at break (%) ≥500 600 GB/T 528
Tensile shear strength (MPa) ≥1.5 2 GB/T 7124
Extrusion rate (ml/min) ≥250 320 GB/T 13477.4

Typical values from the printed catalogue, transcribed as printed. Where the catalogue printed a unit that does not fit the value (density in g/m³), the page shows g/cm³ — see the note below.

Packaging

FormatSizeCarton / unit
cartridge310 ml12 / 20 / 24 pcs
sausage400 / 600 ml20 pcs
barrel200 L / 250 kg—

Where it is used

  • Sealing body skins and aluminium trim panels
  • Bonding and sealing interior body components
  • Edge sealing for doors, tailgates and bonnets
  • Seam sealing on welded body joints
  • Body sealing on converted and specialty vehicles
  • Waterproofing container seams

Further reading

Body seam sealing: sealer, adhesive or both — the guide this model belongs to

Ordering. Send the model, quantity, pack format and destination — we reply with FOB/CIF pricing, lead time and the documents your customs broker will ask for. Email a quote request or write to ryan@pu-karmind.net.